Glennawa et al. have studied the kinetics of thiourea dissolved gold . It is more consistently believed that the rate of gold dissolved in thiourea acidic solution in the presence of oxidant is controlled by the diffusion process and the thiourea is determined. Diffusion coefficient. The galvanic corrosion process of gold dissolved in thiourea acidic solution is shown in Figure 1.
Since the standard oxidation potential difference of gold dissolution is large when dissolved oxygen is used as the oxidant, the speed is mainly controlled by the diffusion process, and the main factor affecting the diffusion is the concentration difference, which obeys Fick's law. Therefore, the diffusion rate of thiourea to the surface of the gold particles in the anode region is: [next]
[next]
According to the above equilibrium concentration of thiourea, and the lower limit of the potential value of thiourea is 0.38V, the pH can be determined to be 1.68. If the concentration of thiourea in the solution is increased, the concentration of dissolved oxygen should be increased correspondingly. When the pH of the medium, such as a thiourea concentration of 0.03 mol, the pH of the medium should be less than 1.29.
Under the optimal conditions, more than 90% of gold can be dissolved in 30 minutes, and 95% of gold can be dissolved in 60 minutes.
Hydraulic Post Driver For Tractor
Hydraulic Post Driver For Tractor,Hydraulic Post Driver Tractor For Fence,Wheeled Hydraulic Post Driver,Tractor Type Hydraulic Post Driver
Yantai Rocka Machinery Co., Ltd , https://www.rockabreaker.com